Polymer Property : Tear Strength = 45.9 kN/m
Polymer Property :
Tear Strength =
45.9 kN/m
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tear Strength
45.9
kN/m
262
pli
as molded- 10 minutes at 116°C; Die B
Multibase SILASTIC® Q7-4750 Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase