Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 44.9 kN/m | 256 pli | Die B, post cured- 4 hours at 177°C; ASTM D624 |
Multibase C6-540 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 44.9 kN/m | 256 pli | Die C; ASTM D624 |
Teknor Apex Monprene® MP-2156-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |