Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 76.5 kN/m | 437 pli | ASTM D412 |
Stellarchem SV-B87E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |