Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 7.70 kN/m | 43.9 pli | Die B |
Momentive Performance Materials RTV8262 Red General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |