Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 7.54 kN/m | 43.0 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3805M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer.. |
|||
Tear Strength | 7.54 kN/m | 43.0 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® ST-6105 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne Firs.. |