Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 74.0 kN/m | 422 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 8 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 74.0 kN/m | 422 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 8 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 74.0 kN/m | 422 pli | DIN 53515 |
Lubrizol ESTANE® 5714F1 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |