Mechanical Properties Metric English Comments
Tear Strength 41.2 kN/m
235 pli
ASTM D624
Multibase Multi-Flex® TPE A 7301 BLK
The data is the actual data obtained from the above sample. This material is based on Shell's Kraton G technology. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 41.2 kN/m
235 pli
ASTM D624
Multibase Multi-Flex® TPE A 8109 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 41.2 kN/m
235 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible R5165A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 41.2 kN/m
235 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 41.2 kN/m
235 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 41.2 kN/m
235 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 41.2 kN/m
235 pli
B-type, Vulcanized
KKPC KOSYN 1712 Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tear Strength 41.2 kN/m
235 pli
B-type, Vulcanized
KKPC KOSYN 1712C Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tear Strength 41.2 kN/m
235 pli
Die C; ASTM D624
Mearthane Durethaneâ„¢ S DS-360A Solid Polyurethane Elastomer
TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
Tear Strength 41.2 kN/m
235 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N550 (FEF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 41.2 kN/m
235 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Oyster Shell Calcium Carbonate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 41.2 kN/m
235 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 41.2 kN/m
235 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 41.2 kN/m
235 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 41.2 kN/m
235 pli
Dow Corning SILASTIC® LC-45-2004 PART A&B KIT
45 Durometer, 2 parts, 1 to 1 mix, translucent, injection molding grade Liquid Silicone Rubber. Fast curing speed, long pot life (72 hours), high transparency, high tear strength, low compression se..
Tear Strength 41.2 kN/m
235 pli
Die C; ASTM D624
Aaron Industries AAROPRENE® ATPR 1000 80A Elastomeric Compound
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
Tear Strength 41.2 kN/m
235 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 41.2 kN/m
235 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 41.2 kN/m
235 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N550 (FEF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 41.2 kN/m
235 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 41.2 kN/m
235 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 41.2 kN/m
235 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-3870E Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionPolyOne First ChoiceDisclaimer: A ther..
Tear Strength 41.2 kN/m
235 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Oyster Shell Calcium Carbonate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..