Mechanical Properties Metric English Comments
Tear Strength 71.0 kN/m
405 pli
Die C; Cross direction; ASTM D624
Teknor Apex Sarlink® 4190 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical..
Tear Strength 71.0 kN/m
405 pli
Die C; Cross direction; ASTM D624
Teknor Apex Sarlink® 4490 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4490 is a medium hardness grade possessing exceptional tensile strength, superior compressio..
Tear Strength 71.0 kN/m
405 pli
unnotched; ASTM D624 (C)
Arkema Group Pebax® 3533 Polyether Block Amide (PEBA)
Information provided by Arkema Group
Tear Strength 71.0 kN/m
405 pli
Die 'C' Tear; 20 in/min; ASTM D624
PolyOne Elastamax XL 0254-15 TPU-Based Thermoplastic Elastomer  (discontinued **)
This is a urethane based thermoplastic elastomer specially lubricated for auto suspension bushings. Physical Form: Pellets. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hann..