Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 7.012 kN/m | 40.01 pli | |
Parker Chomerics CHO-SEAL 1260 Conductive Elastomer Conductive Elastomer. CHO-SEAL 1260 elastomer is a silver-filled-silicone intended for mounting silicon wafers during processes such as ion milling. It provides high levels of electrical and thermal.. |