Polymer Property : Tear Strength = 4.56 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 4.56 kN/m
26.0 pli
Initial Tear Strength; ASTM D624 Die C
Saint-Gobain Korel® K40-20 Medium Deflection Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi..