Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 700 kN/m | 3990 pli | ASTM D624 |
GRECO ISOTHANE 3090AF Polyether TPU Resin ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro.. |
|||
Tear Strength | 700 kN/m | 3990 pli | ASTM D624 |
GRECO ISOTHANE 5090A Polyether TPU Resin ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro.. |