Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 4.90 - 6.86 kN/m | 28.0 - 39.2 pli | ASTM D624 |
Proto3000 Objet Digital Materials™ DM_9510 Rubber-like Prototyping Polymer Primary material: TangoGraySecondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide th.. |
|||
Tear Strength | 4.90 - 6.86 kN/m | 28.0 - 39.2 pli | ASTM D624 |
Proto3000 Objet Digital Materials™ DM_9850/9750 Rubber-like Prototyping Polymer Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structu.. |