Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 38.3 kN/m | 219 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Over-Cured MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 38.3 kN/m | 219 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N220 (ISAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 38.3 kN/m | 219 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N220 (ISAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 38.3 kN/m | 219 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Over-Cured MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |