Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 377 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 66.1 kN/m
377 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 66.0 kN/m
377 pli
with incision; ISO 34B
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Tear Strength 66.0 kN/m
377 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-550 (FEF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 66.1 kN/m
377 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 66.1 kN/m
377 pli
73°F, Die C; ASTM D624
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Tear Strength 66.0 kN/m

@Thickness 0.760 mm
377 pli

@Thickness 0.0299 in
Split tear strength; extruded sheet; ASTM D1938
BASF Elastollan® 1185A10W Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tear Strength 66.0 kN/m

@Thickness 0.760 mm
377 pli

@Thickness 0.0299 in
Split tear strength; extruded sheet; ASTM D-1938
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tear Strength 66.0 kN/m
377 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-550 (FEF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 66.0 kN/m

@Thickness 0.760 mm
377 pli

@Thickness 0.0299 in
Split tear strength; extruded sheet; ASTM D-1938
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tear Strength 66.0 kN/m

@Thickness 0.760 mm
377 pli

@Thickness 0.0299 in
Split tear strength; extruded sheet; ASTM D-1938
BASF Elastollan® 1185A10V Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tear Strength 66.0 kN/m

@Thickness 0.760 mm
377 pli

@Thickness 0.0299 in
Split tear strength; extruded sheet; ASTM D1938
BASF Elastollan® 1185A10Y Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Copyright © lookpolymers.com All Rights Reserved