Mechanical Properties Metric English Comments
Tear Strength 65.7 kN/m
375 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Benzoflex 9-88SG Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 65.7 kN/m
375 pli
Die C; ASTM D624
Teknor Apex Telcar® TL-1183A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tear Strength 65.7 kN/m
375 pli
ASTM D624
Teknor Apex Telcar® TL-1273A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tear Strength 65.7 kN/m
375 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Benzoflex 9-88SG Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 65.7 kN/m
375 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-220 (ISAF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 65.7 kN/m
375 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-220 (ISAF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..