Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 65.6 kN/m | 374 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.20 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 65.6 kN/m | 374 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 5 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 65.5 kN/m | 374 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.25 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 65.6 kN/m | 374 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.20 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 65.6 kN/m | 374 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 5 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 65.5 kN/m | 374 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.25 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |