Polymer Property : Tear Strength = 36.4 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 36.4 kN/m
208 pli
Across Flow; ASTM D624
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tear Strength 36.4 kN/m
208 pli
Flow; ASTM D624
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tear Strength 36.4 kN/m
208 pli
Across Flow; ASTM D624
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tear Strength 36.4 kN/m
208 pli
Flow; ASTM D624
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tear Strength 36.4 kN/m
208 pli
ASTM D624
PolyOne Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t..
Tear Strength 36.4 kN/m
208 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.5 PHR Sulfur
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 36.4 kN/m
208 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.5 PHR Sulfur
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..