Polymer Property : Tear Strength = 356 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 62.4 kN/m
356 pli
Die C; ASTM D624
ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer
Product Description: Vistamaxx 3000 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Technology. It has moderate elastomeric properties, is easy to ..