Polymer Property : Tear Strength = 35.9 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 6.30 - 104 kN/m
35.9 - 593 pli
Average value: 34.6 kN/m Grade Count:26
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Tear Strength 6.30 kN/m
35.9 pli
Trouser, Press-cured 5 minutes at 190°C; DIN 53507
DuPont Vamac® DP HVA-2 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
Tear Strength 6.30 kN/m
35.9 pli
Die C, 510 mm/min; ASTM D624
PolyOne Elastamax™ XL 0141-115 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco..