Tear Strength 0.540 kN/m
3.08 pli
Die C; ASTM D624
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, High-Resilience, Higher density
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Tear Strength 0.540 kN/m
3.08 pli
Die C; ASTM D624
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, Viscoelastic
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.