Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 3.06 kN/m | 17.5 pli | |
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1.. |
|||
Tear Strength | 3.06 kN/m | 17.5 pli | |
DuPont Performance Polymers Kalrez® 1050LF FFKM Perfluoroelastomer A general-purpose compound for O-rings, seals, and other parts used in chemical process industries. It has good hot water/steam, excellent amine resistance, and enhanced compression set properties... |
|||
Tear Strength | 3.06 - 168 kN/m | 17.5 - 959 pli | Average value: 24.5 kN/m Grade Count:89 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |