Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 4.91 - 51.9 kN/m | 28.0 - 296 pli | Average value: 17.4 kN/m Grade Count:181 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |