Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 51.2 kN/m | 292 pli | Die B,post cured- 2 hours at 166°C; ASTM D624 |
Multibase SILASTIC® 7-6860 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 51.2 kN/m | 292 pli | |
Dow Corning SILASTIC® LC-60-2004 PART A&B KIT 60 Durometer, 2 parts, 1 to 1 mix, translucent, FDA 21 CFR 177.2600 and BfR, XV, molding and injection molding grade Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Tear Strength | 51.1 kN/m | 292 pli | |
3M Scotchkote™ 80XRG 539 Urethane Elastomer Scotchkote Urethane Elastomer 80XRG 539 has been specifically developed as a fast curing elastomeric repair system with a high degree of flexibility for rebuilding and resurfacing rubber components... |