Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 20.0 - 29.4 kN/m | 114 - 168 pli | Average value: 24.9 kN/m Grade Count:9 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |