Mechanical Properties Metric English Comments
Tear Strength 49.8 kN/m
284 pli
Die B, post cured- 4 hours at 177°C; ASTM D624
Multibase C6-570 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 49.7 kN/m
284 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Soft Clay
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 49.7 kN/m
284 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Soft Clay
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..