Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 49.061 kN/m | 279.87 pli | |
Dow Corning SILASTIC® 9280/60E KIT PARTS A&B 75 Shore A hardness, two-part, 1 to 1 mix, translucent, injection molding grade Liquid Silicone Rubber.Information provided by Dow Corning |