Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 48.6 kN/m | 277 pli | Die B,post cured- 2 hours at 200°C; ASTM D624 |
Multibase SILASTIC® Q7-4850 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 48.6 kN/m | 277 pli | ISO 34 |
Multibase TPSiV® 4200-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Tear Strength | 48.5 kN/m | 277 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4725P General Purpose Molding FormulationNordel® IP 4725P |