Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.60 - 275 kN/m | 9.13 - 1570 pli | Average value: 34.8 kN/m Grade Count:448 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |