Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 4.22 kN/m | 24.1 pli | |
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |