Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 231 kN/m | 1320 pli | |
Dow Corning D94-20P A&B KIT Two-part, 1:1 ratio, addition cure silicone elastomer for automated assembly of integrated compression sealsInformation provided by Dow Corning |