Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 3.00 - 39.4 kN/m | 17.1 - 225 pli | Average value: 11.2 kN/m Grade Count:45 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |