Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 21.4 kN/m | 122 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 21.4 kN/m | 122 pli | post cured- 8 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4780 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 21.4 kN/m | 122 pli | Press-cured 5 minutes at 190°C; ISO 34 |
DuPont Vamac® DP DIAK No. 7 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |