Polymer Property : Tear Strength = 2070 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 363 kN/m
2070 pli
MD; ASTM D1922
LG Chemical LUTENE FB0300 LDPE Blown Film Grade
Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e..