Polymer Property : Tear Strength = 2.94 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 2.94 - 4.90 kN/m
16.8 - 28.0 pli
ASTM D624
Proto3000 Objet TangoBlack FullCure970 Rubber-like Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..