Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 2.50 kN/m | 14.3 pli | |
ACC MM816 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Tear Strength | 2.50 kN/m | 14.3 pli | |
ACC MM820 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |