Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 2.075 kN/m | 11.84 pli | BS EN ISO 8067 1995 |
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |