Mechanical Properties Metric English Comments
Tear Strength 185 kN/m
1060 pli
Graves (initial), TD; ASTM D1004
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o..
Tear Strength 185 kN/m
1060 pli
ASTM D624
C.O.I.M. LARIPUR® LPR6650 Modified Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..