Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 3.16 kN/m | 18.0 pli | Die C; ASTM D624 |
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer This two-component polyurethane casting system makes type of soft elastomer material known as “gel”. Applications for this material include filling component for computer keyboard/mouse-pad wrist.. |
|||
Tear Strength | 3.16 kN/m | 18.0 pli | Die C; ASTM D624 |
Monmouth Rubber & Plastics Durafoamâ„¢ C41 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |