Polymer Property : Tear Strength = 179 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 179 kN/m
1020 pli
without incision; ISO 34B
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in..
Tear Strength 179 kN/m
1020 pli
without incision; ISO 34B
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 179 kN/m
1020 pli
Die C; ASTM D624
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in..