Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 285 kN/m | 1630 pli | ASTM D624 |
BASF Elastollan® S74D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |