Mechanical Properties Metric English Comments
Tear Strength 263 kN/m
1500 pli
Die C; ASTM D624
Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.