Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 26.03 kN/m | 148.7 pli | |
Microcell Composite Company CELLAMP® 5000 Pellets CELLAMP® Pellets can be used for producing foaming boards with damping properties, which yield the best efficiency between -10°C and room temperature.Information provided by Microcell Composit.. |