Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 146 kN/m | 833 pli | ISO 34B |
Huntsman AVALON® 95 AB Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Tear Strength | 146 kN/m | 833 pli | Graves (initial), TD; ASTM D1004 |
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Tear Strength | 146 kN/m | 833 pli | ISO 34B |
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |