Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 241 kN/m | 1380 pli | ASTM D1004 |
Radici Heraflex® E 6521 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Medium-high Modulus, Nominal Shore D/15s 57. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |