Mechanical Properties Metric English Comments
Tear Strength 64.9 - 237 kN/m
370 - 1350 pli
Average value: 134 kN/m Grade Count:4
Overview of materials for Polycarbonate-Urethane
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr..