Polymer Property : Tear Strength = 108 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 87.3 - 108 kN/m
498 - 616 pli
Initial Tear Strength; ASTM D-1004
Saint-Gobain Norton® FEP Fluoropolymer Film
Features/Benefits:Outstanding clarityOutstanding anti-stick release propertiesPerformance from -254°C (-425°F) to 205°C (400°F)Exceptional chemical resistance and electric propertiesComp..