Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.90 kN/m | 10.9 pli | JIS K6301-B |
Stellarchem MP-855WR TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |