Tear Strength 1.75 kN/m
10.0 pli
Split; ASTM D624
Northstar Polymers MPP-A65A High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Tear Strength 1.76 kN/m
10.0 pli
JIS K6301-B
Stellarchem GP-930 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Tear Strength 1.75 kN/m
10.0 pli
Initial Tear Strength
Saint-Gobain CHR® K104 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..