Mechanical Properties Metric English Comments
Tear Strength 0.789 kN/m
4.50 pli
Dow Corning 9601 TEXTILE PRINTING INK
Specifically for fluorosilicone peroxide cured rubber adhesion to generic metals, glass, fabrics, and ceramicsInformation provided by Dow Corning