Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.701 kN/m | 4.00 pli | Split Tear Resistance |
Northstar Polymers MPS-F04A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |